Inconel 660 / Alloy 660 (UNS S66286 / SUH660 / GH2132) – U'amea Fa'ama'a'a e Fa'avae i le U'amea Sili mo le Auaunaga i le Vevela Maualuga

Fa'amatalaga Pupuu:

Inconel 660 (UNS S66286 / SUH660 / GH2132 /Numera o le Itulagi. 1.4980) o se u'amea e fa'avae i luga o le u'amea e mafai ona fa'ama'a'aina i le vaipuna ma e matua'i malosi lava i le vevela maualuga ma tete'e atu i le 'okesaita e o'o atu i le 704°C (1300°F). E sapalai e le Womic Steel le Inconel 660 i le tele o ituaiga oloa e aofia ai paipa seamless, paipa uelo, u'amea pa, u'amea plate, u'amea coil, strip, flanges, fittings, forgings, wire, ma fa'amau mo le aerospace, gas turbine, ta'avale, fa'aniukilia, ma petrochemical applications.


Fa'amatalaga o le oloa

Fa'ailoga o Oloa

O le ā le Inconel 660?

O le Inconel 660 o se u'amea e fa'avae i le nickel-chromium superalloy e fa'amalosia e ala i le fa'aputuina o le γ' [Ni₃(Al,Ti)] phase i le taimi o le fa'avevela. O le u'amea e aofia ai le tusa ma le 24-27% nickel, 13.5-16% chromium, ma fa'aopoopoga o le titanium (1.9-2.35%), alumini (0.10-0.35%), molybdenum (1.0-1.5%), ma le vanadium (0.10-0.50%). Ua mamanuina mo fa'aoga e mana'omia ai le malosi maualuga e o'o atu i le 700°C ma le tete'e lelei i le oxidation ma le ele.

Ua lauiloa le Vasega 660 mo:

●Malosiaga o le vevela maualugae oo atu i le 704°C (1300°F)

●Tete'e lelei tele i le malepei le vevela maualuga

●E mafai ona fa'ama'a'a le timugae ala i togafitiga vevela masani o le matua

●Tete'e lelei i le fa'a'okesae oʻo atu i le 815°C

●Tete'e atu i le fa'amalieina o le atuatuvalei le vevela maualuga

●E lē fa'amanetameatotino

●Lelei le faiga o le lalagainama le faigofie ona fa'aaogaina

Fa'atulagaga Fa'akemikolo

Elemene UNS S66286 (ASTM) SUH660 (JIS) GH2132 (GB) Matafaioi
Nickel (Ni) 24.0 – 27.0 24.0 – 27.0 24.0 – 27.0 Fa'amautu Austenite, tete'e atu i le 'ele
Kromium (Cr) 13.5 – 16.0 13.5 – 16.0 13.5 – 16.0 Tete'e i le oxidation, carbide former
Molibdenum (Mo) 1.0 – 1.5 1.0 – 1.5 1.0 – 1.5 Fa'amalosia o fofo mautu
Titanium (Ti) 1.90 – 2.35 1.90 – 2.35 1.90 – 2.35 timuga o le γ', fa'ama'a'aina o le matua
Alumini (Al) 0.10 – 0.35 ≤ 0.35 ≤ 0.35 timuga γ'
Vanadium (V) 0.10 – 0.50 0.10 – 0.50 0.10 – 0.50 Fa'amamāina o saito, fa'aputuga carbide
Boron (B) 0.003 – 0.010 0.001 – 0.010 0.001 – 0.010 Fa'amalosia o tuaoi o fatu
Kobalti (Ko) ≤ 1.00 ≤ 1.00 ≤ 1.00 Elemene totoe
U'amea (Fe) Paleni Paleni Paleni Elemene autū
Kaponi (C) ≤ 0.08 ≤ 0.08 ≤ 0.08 Mea fa'asolo o le carbide
Silikoni (Si) ≤ 1.00 ≤ 1.00 ≤ 1.00 Mea e aveese ai le okesene
Manganese (Mn) ≤ 2.00 ≤ 2.00 ≤ 2.00 Mea e aveese ai le okesene
Fosforus (P) ≤ 0.025 ≤ 0.040 ≤ 0.030 Le mama
Sulfur (S) ≤ 0.025 ≤ 0.030 ≤ 0.020 Le mama

Meatotino Fa'amekanika

Tulaga ua Fa'a'aisa (Ua Togafitia le Vaifofo)

Meatotino ASTM A453 Vasega 660 Taua
Malosiaga o le Fetaia'i ≤ 724 MPa (105 ksi)  
Malosiaga o le Gaosiga (0.2% Offset) –  
Fa'aloloa ≥ 25%  
Faigata ≤ 91 HRB

Tulaga Matua (Ua Fa'ama'a'aina le Timuga)

Meatotino ASTM A453 Vasega 660 Ausia Masani
Malosiaga o le Fetaia'i ≥ 965 MPa (140 ksi) 1,000 – 1,100 MPa
Malosiaga o le Gaosiga (0.2% Offset) ≥ 655 MPa (95 ksi) 700 – 800 MPa
Fa'aloloa ≥ 15% 18 – 25%
Faigata 24 – 35 HRC 28 – 32 HRC
Malosiaga o le Totolo (650°C, 100h) ≈ 240 MPa  
Malosiaga o le Totolo (700°C, 100h) ≈ 210 MPa

Meatotino Faaletino

Meatotino Taua
Mafiafia 7.95 kalama/cm³
Fa'asologa o le Liusuavai 1371 – 1427°C
Fa'avevela o le Tafega 15.0 W/m·K i le 150°C
Fa'atusatusaga o le Fa'alauteleina o le Vevela 16.8 × 10⁻⁶/°C (20-100°C)
Modulus Fa'alelei 201 GPa
Malosiaga Fa'amagnetika E lē fa'amaneta

Fa'amanuiaga Autū o le Inconel 660

Malosiaga o le Vevela Maualuga– E faatumauina e le Inconel 660 le malosi maualuga i le tensile, le vaivai, ma le creep-rupture e oo atu i le 704°C. O le γ' precipitation strength mechanism e maua ai le malosi sili atu i le vevela maualuga pe a faatusatusa i u'amea stainless austenitic masani. E masani ona faaaogaina le alloy mo turbine bolts ma fixtures lea e taua tele ai le tete'e atu i le relaxation.

Tete'e Sili Ona Lelei i le Malepelepe– E iai le tete'e mata'ina o le u'amea i le vevela maualuga. E sili atu i le 1,000 itula le umi e ola ai i le vevela e pei o le sosolo i le 650°C i lalo o le mamafa feololo, ma avea ai ma mea e fa'atuatuaina mo galuega fa'atino i le vevela maualuga mo se taimi umi.

Tete'e Lelei i le Oxidation ma le Corrosion– Faatasi ai ma le 13.5-16% o le chromium, e maua ai e le Inconel 660 le tete'e lelei i le fa'a'okesaita, fa'apalapala, ma le 'ele i le vevela maualuga. E lelei le fa'atinoga o le 'au'au i siosiomaga fa'a'okesaita e o'o atu i le 815°C ma tete'e atu i le tele o mea 'ele.

E mafai ona fa'ama'a'aina le timuga– E mafai ona fa'ama'a'aina le Inconel 660 i le vaipuna e ala i le fa'avevela o le tino. O le ta'amilosaga masani o le tino (675-705°C, 12-16 itula) e atiina ae ai meatotino fa'ainisinia sili ona lelei ma maua ai le tete'e lelei i le fa'aitiitia o le mamafa, lea e taua tele mo fa'aoga fa'amau.

Tete'e Lelei i le Vaivai– E ofoina atu e le u'amea fa'afefiloi le tete'e lelei i le vaivai ma le vevela, ma e talafeagai ai mo vaega e feagai ma le uta fa'asolosolo i le vevela maualuga. E taua tele lenei mea mo fa'aoga turbine ma vaega o le afi.

Lelei tele le Faigofie ona Galue ma le Masini– E sili atu le faigofie ona fa'aaogaina le Inconel 660 nai lo le tele o isi superalloys. E faigofie ona fa'apala, galue i le vevela, ma galue i le malulu. E mafai ona fa'apipi'i le alloy e fa'aaoga ai le TIG, MIG, ma le fa'apipi'iina o le tete'e ma u'amea fa'atumu talafeagai.

Fa'amanuiaga Autū o le Inconel 660

Malosiaga o le Vevela Maualuga– E faatumauina e le Inconel 660 le malosi maualuga i le tensile, le vaivai, ma le creep-rupture e oo atu i le 704°C. O le γ' precipitation strength mechanism e maua ai le malosi sili atu i le vevela maualuga pe a faatusatusa i u'amea stainless austenitic masani. E masani ona faaaogaina le alloy mo turbine bolts ma fixtures lea e taua tele ai le tete'e atu i le relaxation.

Tete'e Sili Ona Lelei i le Malepelepe– E iai le tete'e mata'ina o le u'amea i le vevela maualuga. E sili atu i le 1,000 itula le umi e ola ai i le vevela e pei o le sosolo i le 650°C i lalo o le mamafa feololo, ma avea ai ma mea e fa'atuatuaina mo galuega fa'atino i le vevela maualuga mo se taimi umi.

Tete'e Lelei i le Oxidation ma le Corrosion– Faatasi ai ma le 13.5-16% o le chromium, e maua ai e le Inconel 660 le tete'e lelei i le fa'a'okesaita, fa'apalapala, ma le 'ele i le vevela maualuga. E lelei le fa'atinoga o le 'au'au i siosiomaga fa'a'okesaita e o'o atu i le 815°C ma tete'e atu i le tele o mea 'ele.

E mafai ona fa'ama'a'aina le timuga– E mafai ona fa'ama'a'aina le Inconel 660 i le vaipuna e ala i le fa'avevela o le tino. O le ta'amilosaga masani o le tino (675-705°C, 12-16 itula) e atiina ae ai meatotino fa'ainisinia sili ona lelei ma maua ai le tete'e lelei i le fa'aitiitia o le mamafa, lea e taua tele mo fa'aoga fa'amau.

Tete'e Lelei i le Vaivai– E ofoina atu e le u'amea fa'afefiloi le tete'e lelei i le vaivai ma le vevela, ma e talafeagai ai mo vaega e feagai ma le uta fa'asolosolo i le vevela maualuga. E taua tele lenei mea mo fa'aoga turbine ma vaega o le afi.

Lelei tele le Faigofie ona Galue ma le Masini– E sili atu le faigofie ona fa'aaogaina le Inconel 660 nai lo le tele o isi superalloys. E faigofie ona fa'apala, galue i le vevela, ma galue i le malulu. E mafai ona fa'apipi'i le alloy e fa'aaoga ai le TIG, MIG, ma le fa'apipi'iina o le tete'e ma u'amea fa'atumu talafeagai.

Togafitiga Fa'avevela o Inconel 660

O le Inconel 660 o se uʻamea faʻamaʻaʻa e mafai ona faʻamaʻaʻaina e manaʻomia ai togafitiga faʻapitoa o le vevela e ausia ai meatotino faʻainisinia sili ona lelei:

Fa'asusuina o le Vai (Tulaga A):

●Vevela:980 – 1010°C (1800 – 1850°F)

●Taimi e Fa'asusu ai:1 itula

●Fa'amālūlūina:Fa'amālūlū vave (fa'amālūlūina o le suāuu po'o le vai)

●Fa'amoemoega:Fa'ata'ape'ape uma mea e maua mai ai, maua le austenite e tasi le vaega

●I'uga:Tulaga vaivai, e mafai ona galue, ua sauni mo le fausiaina ma le masiniina

Fa'ama'a'aina o le Timuga (Matua – Tulaga B):

●Vevela:675 – 705°C (1250 – 1300°F)

●Taimi e Fa'asusu ai:12 – 16 itula

●Fa'amālūlūina:Malūlū le ea

●Fa'amoemoega:Pepa Ni₃(Al,Ti) γ' e fa'amalosi

●I'uga:Malosi sili ona maualuga ma le tete'e atu i le totolo

Matua Faalua (Suiga):

● Vaega Muamua: 705°C mo le 16 itula, fa'amālūlū le ogaumu i le 620°C

● Vaega Lua: 620°C mo le 16 itula, fa'amālūlū i le ea

●Fa'amoemoega:Fa'aleleia le tete'e atu i le fa'aitiitia o le atuatuvale mo fa'aoga fa'amau

Pepa o Oloa o lo'o Maua mai Womic Steel

Paipa e leai se Su'isu'i & Paipa e leai se Su'isu'i

●Lapoa i fafo:6mm – 200mm

●Mafiafia o le Puipui:1mm – 25mm

●Umi:E oo atu i le 12m

●Tulaga Faatonuina:ASTM B639, ASTM B983, AMS 5731, AMS 5732, AMS 5737, AMS 5895

●Talosaga:Paipa fa'agasolo vevela maualuga, paipa fesuia'i vevela, laina meafaigaluega, paipa va'alele

●Upu autu:Paipa Inconel 660 e leai se so'oga, paipa Vasega 660, paipa UNS S66286, paipa SUH660, paipa e leai se so'oga 1.4980

U'amea (Lapotopoto, Fa'atafafā, Mafolafola, Hex)

●Lapoa:6mm – 300mm

●Luga:Fa'a'ofu vevela, Susulu (fa'a'ofu malulu), Eleele, Liliu

●Tulaga Faatonuina:ASTM A453, ASTM B639, AMS 5731, AMS 5732, AMS 5734, AMS 5737

●Talosaga:Poloti turbine, mea fa'amau, pine, au, 'au o le valve, mea fa'amekani

●Upu autu:Pa la'au lapotopoto Inconel 660, Pa vasega 660, U'amea SUH660, ASTM A453 Vasega 660, fa'amau vevela maualuga

Ipu ma Pepa U'amea

●Mafiafia:1mm – 100mm

●Lautele:E oo atu i le 2000mm

●Tulaga Faatonuina:AMS 5525, AMS 5858

●Talosaga:Vaega o le va'a mamafa, vaega fa'atulagaina, avanoa flange

●Upu autu:Ipu Inconel 660, pepa Vasega 660, ipu u'amea, ipu vevela maualuga

U'amea Coil & Strip

●Mafiafia:0.5mm – 4.0mm

●Lautele:10mm – 1000mm

●Tulaga Faatonuina:AMS 5525

●Talosaga:Vaega ua faia, mea e fa'apupuna ai le afi, fa'ailoga

●Upu autu:Inconel 660 coil, fasipepa, fasipepa vevela maualuga

Flanges ma Mea Fa'apipi'i

●Ituaiga:Ua Fa'apipi'i, Mase'e, Tauaso, Fa'apipi'i Socket, Fa'a'ofuofu

●Tele:1/2" – 24"

●Fua Fa'atatau o le Mamafa:Vasega 150 – Vasega 2500

●Tulaga Faatonuina:ASTM A453, ASME B16.5

●Upu autu:Inconel 660 flanges, Vasega 660 mea fa'apipi'i

Fa'a'ole'ole

●Ituaiga:Mama, tisiketi, au, tino o valve, fausaga fa'apitoa

●Mamafa:E oo atu i le 3,000kg i le fasi pepa

●Tulaga Faatonuina:ASTM A453, AMS 5731

●Upu autu:Inconel 660 forging, forged ring, turbine component forging

Fa'amau (Pulu, Nati, Fa'amau)

●Ituaiga:Polo fa'amau hex, Sikulima tapuni ulu soketi, Polo fa'amau fa'amau, U'amea fa'apipi'i, Nati, Masini fa'amama

●Tele:M2 – M100, 1/4" – 4"

●Tulaga Faatonuina:ASTM A453 Vasega 660, ASTM B637

●Talosaga:Polo o turbine, feso'ota'iga o le flange vevela maualuga, fa'amau fa'atulagaina

●Upu autu:Fa'amau Inconel 660, Fa'amau fa'amau vasega 660, fa'amau fa'amau vevela maualuga, fa'amau turbine

Valves Vasega 660

●Ituaiga:Vali polo, Vali faitotoa, Vali lalolagi, Vali siaki

●Tele:1/2" – 12"

●Fua Fa'atatau o le Mamafa:Vasega 150 – Vasega 2500

●Fa'asologa o le Vevela:-196°C i le +704°C

●Tulaga Faatonuina o le Fuafuaga:API 608, API 6D, ASME B16.34

●Fa'agaioiga:Tusia, Pneumatic, Eletise

●Talosaga:Fa'aesea o le fa'agasologa o le vevela maualuga, laina ausa o le turbine, puleaina o le turbine kesi

Vasega 660 vs. Inconel 718: Fa'atusatusaga

O le Inconel 660 ma le Inconel 718 o ni superalloys e fa'ama'a'a ai le precipitation, ae e iai ni eseesega manino:

Inconel 660 – U'amea Fa'avae i le Vevela Maualuga

●Elemene Faavae:U'amea (paleni) ma le 24-27% Ni

●Vaega o le fa'amalosia:γ' (Ni₃(Al,Ti))

●Malosiaga o le Fetaia'i (matua):≥ 965 MPa

●Malosiaga o le vevela:E oo atu i le 704°C

●Fa'aoga autū:Poloti turbine, mea fa'amau, pine, vaega o le afi vaalele

●Tau:E sili atu le taugofie nai lo le 718 e fa'avae i le nickel

●Inconel 718 – U'amea Fa'apitoa e Fa'avae i le Nickel

●Elemene Faavae:Nikel (50-55%) fa'atasi ai ma le 18-20% Fe

●Vaega o le fa'amalosia:γ' (Ni₃Al) + γ'' (Ni₃Nb)

●Malosiaga o le Fetaia'i (matua):≥ 1,240 MPa

●Malosiaga o le vevela:E oo atu i le 700°C

●Fa'aoga autū:Tisiketi turbine, afi roketi, suau'u ma kesi HPHT

O afea e filifili ai le Vasega 660:Talosaga e manaʻomia ai le faʻamau ma le faʻamauina i le vevela maualuga, vaega o le afi vaalele, faʻamau o turbine, ma taʻavale faʻatinoga maualuga lea e taua ai le tau ma e manaʻomia ai le malosi maualuga e oʻo atu i le 700°C.

O afea e filifili ai le Inconel 718:Talosaga e manaʻomia ai le malosi maualuga i le vevela maualuga, le malōlō i le gau, ma le teteʻe atu i le totolo i le vevela e oʻo atu i le 700°C lea e itiiti ai le tau.

Tulaga Faatonuina ma Fa'amatalaga

Tulaga Masani Fa'amatalaga
Fa'ailoga a le UNS S66286
Numera o Werkstoff 1.4980
AISI/SAE 660
ASTM A453 Fa'amatalaga masani mo le fa'amauina i le vevela maualuga
ASTM B639 Pa/tootoo u'amea vevela maualuga
AMS 5525 Ipu/pepa/la'ei
AMS 5731 Pa, uaea, mea e fa'apala ai
AMS 5732 Pa, uaea, mea e fa'apala ai
AMS 5734 Pa, uaea, mea e fa'apala ai
AMS 5737 Paipa ma le paipa
AMS 5895 Pa, uaea, mea e fa'apala ai
JIS SUH660
GB/T GH2132
Europa 1.4980 / X6NiCrTiMoV25-15-2
ISO X6NiCrTiMoV25-15-2

Fa'aoga o Inconel 660

Vaalele– E fa'aaogā tele le Inconel 660 i vaega o le afi vaalele ma le turbine kesi e aofia ai poloti turbine, tisiketi compressor, pusa turbine, vaega afterburner, thrust reversers, ma masini fa'apipi'i afi. O lona tu'ufa'atasiga o le malosi maualuga i le vevela, tete'e atu i le vaivai, ma le tete'e atu i le oxidation e avea ai ma mea lelei mo fa'aoga taua i vaalele. O le u'amea fa'afefiloi o mea masani ia mo poloti ma fa'amau o le afi vaalele e fa'agaoioia i le vevela e o'o atu i le 700°C.

Fa'atupuina o le Malosiaga o Turbine Kesi– O le u'amea fa'a'au'au e fa'aaogaina mo poloti turbine, studs, ma fa'amau i turbine kesi fa'apisinisi, turbine ausa, ma la'au eletise fa'atasi. O lona tete'e atu i le fa'aitiitia o le mamafa i le vevela maualuga e fa'amautinoa ai le fa'atuatuaina o feso'ota'iga fa'amau e ala i le fa'alauteleina o le ola tautua.

Ta'avale– E fa'aaogaina le Inconel 660 i totonu o pusa turbocharger, paipa e alu ese ai le ea, vaega o le afi diesel, ma mea fa'amau e fa'aleleia atili ai le fa'atinoga o ta'avale. O lona gafatia e tete'e atu i le vevela o le kesi alu ese ma le fa'asolosolo o le vevela e talafeagai ai mo afi fa'aonaponei e maualuga le fa'atinoga ma afi turbocharged.

Malosiaga Faaniukilia– O le u'amea fa'afefiloi e fa'aaogaina i vaega o le reactor faaniukilia, totonugalemu o totonu, faiga o le control rod, ma mea fa'amau e maualuga le vevela e mana'omia ai le fa'atuatuaina mo se taimi umi ma le tete'e atu i le neutron irradiation.

Fa'agasologa o le Petrochemical– E fa'aaogaina le Inconel 660 i reactors vaila'au e maualuga le vevela, paipa toe fa'aleleia, vaega o le ogaumu, ma paipa fa'agasolo e mana'omia ai le malosi ma le tete'e atu i le fa'ama'i i le vevela maualuga.

Fa'amauina o le Vevela Maualuga– O le Vasega 660 o le mea masani lea mo fa'aoga fa'amau i le vevela maualuga. O polo ma pine ASTM A453 Vasega 660 e fa'apitoa lautele mo flanges o va'a mamafa, pusa turbine, ma feso'ota'iga paipa vevela maualuga e mana'omia ai le tete'e atu i le totolo ma le fa'aitiitia o le mamafa.

Fesili e Masani Ona Fesiligia

S: O le ā le Inconel 660?

A: O le Inconel 660 (UNS S66286 / SUH660 / GH2132) o se u'amea e fa'ama'a'a ai le precipitation ma e matua'i malosi i le vevela maualuga e o'o atu i le 704°C. E fa'amalosia e le γ' precipitation e ala i le fa'avevela tuai ma e fa'aaogaina lautele mo polo turbine, fa'amau, ma vaega o le afi vaalele.

O le a le eseesega i le va o le Vasega 660 ma le Inconel 718?

A: O le Inconel 660 e fa'avae i le u'amea (fa'atasi ai ma le 24-27% Ni, paleni Fe) ma le malosi fa'ase'e ≥ 965 MPa, ae o le Inconel 718 e fa'avae i le nickel (50-55% Ni) ma le malosi fa'ase'e ≥ 1,240 MPa. O le vasega 660 e sili atu ona taugofie ma fa'aaogaina lautele mo le fa'amauina o polo; O le Inconel 718 e fa'aaogaina mo fa'aoga sili ona malosi.

S: O le a le vevela aupito maualuga e mafai ona fa'aaogaina mo le Inconel 660?

A: Ua fa'atulagaina le Inconel 660 mo le tautua faifai pea e o'o atu i le 704°C (1300°F). Mo le tete'e atu i le 'okesene, e mafai ona fa'asolosolo pu'upu'u e o'o atu i le 815°C (1500°F). E fa'aitiitia tele le malosi o le totolo pe a sili atu i le 700°C.

F: E faigofie ona fa'apipi'i le Inconel 660?

A: Ioe, e mafai ona fa'apipi'i le Inconel 660 e ala i le fa'aaogaina o faiga fa'apipi'i TIG, MIG, ma le tete'e. Peita'i, o le fa'apipi'iina e mana'omia ai le pulea lelei o le vevela e ulufale mai ma le filifiliga o u'amea fa'atumu ina ia 'alofia ai le māvaevae o le vevela. Atonu e mana'omia le fa'amamago ma le fa'amatuaina o le vaila'au pe a uma ona fa'apipi'i e toe fa'afo'isia ai meatotino fa'amekanika.

O a ni mea e tutusa ma le Inconel 660 i le gagana Saina?

A: O le tutusa faa-Saina o le Inconel 660 o le GH2132 (高温合金) mo galuega tau va'alele ma le vevela maualuga, ma o le mea e tutusa ma Iapani o le SUH660.

S: O a ituaiga oloa o lo'o avanoa mo Inconel 660?

A: E sapalai e le Womic Steel le Inconel 660 i paipa e leai ni so'oga, paipa ua fa'apipi'iina, u'amea pa, u'amea laulau, u'amea uaea, u'amea uaea, fusi u'amea, flanges, mea fa'apipi'i, mea fa'apipi'i, uaea, mea fa'amau, ma valves. O fa'amatalaga atoa o oloa ma lapopo'a o lo'o lisiina i le vaega o lo'o maua ai oloa.

F: E manaʻomia ea e le Inconel 660 le togafitiga faʻavevela?

A: Ioe. E manaʻomia e le Inconel 660 le faʻamālūlūina o le vai (980-1010°C) ona sosoo ai lea ma le faʻamaʻaʻaina (675-705°C mo le 12-16 itula) ina ia maua ai ni meatotino faʻainisinia sili ona lelei. O le togafitiga faʻamaʻaʻaina e faʻaosofia ai le vaega γ' mo le faʻamalosia.

Fa'afeso'ota'i le Womic Steel

Upega Tafaʻilagi: www.womicsteel.com
Imeli: sales@womicsteel.com

Telefoni / WhatsApp / WeChat:

Victor: +86 15575100681

Siaki: +86 18390957568

Womic Steel – O lau pa'aga fa'atuatuaina mo paipa Inconel 660 / Vasega 660 (UNS S66286, SUH660, GH2132), u'amea u'amea, u'amea uamea, u'amea uamea, flanges, mea fa'apipi'i, mea e fa'apala ai, ma mea e fa'amau ai mo va'alele, turbine kesi, gaosiga o le eletise, ma fa'aoga fa'amau i le vevela maualuga i le lalolagi atoa. O lo'o maua le su'esu'ega atoatoa, fa'amaoniga a le sosaiete fa'avasega, ma pepa fa'amaonia EN 10204 Type 3.1/3.2.